EPT Retardant Chlorinated paraffin EPT 70% for Conveyor Belting
1.Technical Index
Item Tested | Index |
Chlorine content %, | 70 plusmn2 |
Acid Value (mgKOH/g),oC | .35max |
Carbon Tetrachloride Hangzhou everpower4 microg/g | non |
Softening level (oC), | ge 90 |
Thermal Decomposition Temperature, oC | 170 min |
Warmth Balance Index, (170oC, WeigEPT Decline unEPT4 Hour Heating),% | .3 max |
WeigEPT loss, % | .3 max |
Particle size | twenty mesh sieve passed |
two.Software
(1) Employed as a secondary plasticizer in PVC Resins,Plasticizers ExtenEPTin artificial rubber,Chlorianted Rubber,Nitrocellulose Polystyrene etc….
(two) Employed as EPT Retardant Additive in the manufacturer of Rubber Conveyer Belt,FR Coating (Paint),Cable Components…..
3.Package, transportation and storage
Package: 25kg/craft bag on pallet,18 metric ton for each 20’container
Transportation: the product is of dangerous 1, which should be protected from moist, rainfall and bundle injury in transportation.
Storage: at dry warehouse with excellent ventilation.